Qualification Note
Note: Heat input controls weld cooling rate, which affects HAZ properties, grain size, and toughness. Higher HI = slower cooling = softer HAZ but potentially lower toughness.

Reference

Heat Input = (V x I x 60) / (Travel Speed x 1000) [kJ/in] ASME IX QW-409.1: HI is supplementary essential when impact testing required AWS D1.1: Typically +/-25% of PQR value API 1104: Typically +/-20% of PQR value